| Pipe Conditioning |
1
Surface sandblasting or brushing to get an SAE 2.5 pipe surface.
|
2
Primer application
|
| Rope Insertion
|
3
Wrap the Kevlar rope around the pipe damaged
section. Make sure there is no more than 2mm
gap between 2 successive coils, and tighten strongly
the ends.
|
| Shell assembling |
4
Assemble together the modules that shape the shell regarding the pipe diameter.
|
| Formwork Installation |
5
Put the shell around the rope coils.
|
6
Seal the sides using adhesive tape between the shell and the tube, this way it will prevent any leak of resin.
|
7
Wrap polyethylene film around the shell to make the formwork hermetic.
|
| Resin preparing and injection |
8
Prepare and mix the resin.
|
9
Pour the resin inside the sleeve until fill it, and then let it cure between 2 and 6 hours.
|